Characteristics of Schottky contacts on n-type 4H-SiC using IrO2 and RuO2 SCIE SCOPUS

Title
Characteristics of Schottky contacts on n-type 4H-SiC using IrO2 and RuO2
Authors
Han, SYLee, JL
Date Issued
2003-11-01
Publisher
AMER INST PHYSICS
Abstract
Thermally stable Schottky contacts on n-type 4H-SiC with high Schottky barrier height were demonstrated by annealing the rare earth metal contacts (Ir and Ru) under O-2 ambient. The formation of rare earth metal oxides (IrO2 and RuO2) after O-2 annealing led to the increase of Schottky barrier height (>1.9 eV) and a low reverse leakage current (similar to10(-9) A/cm(2)). Synchrotron radiation photoemission spectroscopy showed that the work function of IrO2 is higher about 0.23 eV than that of Ir and the binding energies of Si 2p and C 1s shifted toward lower binding energies by 0.12 eV in both O-2 and N-2 annealed samples. The oxidation annealing caused predominant Si outdiffusion to the IrO2 (RuO2), leaving Si vacancies behind, leading to the shift of surface Fermi level to the energy level of Si vacancy. Both the formation of oxide and the Fermi level movement played a role in forming the Schottky contact with high barrier height and excellent thermally stability. (C) 2003 American Institute of Physics.
URI
https://oasis.postech.ac.kr/handle/2014.oak/10524
DOI
10.1063/1.1615701
ISSN
0021-8979
Article Type
Article
Citation
JOURNAL OF APPLIED PHYSICS, vol. 94, no. 9, page. 6159 - 6166, 2003-11-01
Files in This Item:

qr_code

  • mendeley

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher

이종람LEE, JONG LAM
Dept of Materials Science & Enginrg
Read more

Views & Downloads

Browse