DC FieldValueLanguage
dc.contributor.authorLee, S.G.-
dc.contributor.authorLee, D.H.-
dc.contributor.authorSohn, S.S.-
dc.contributor.authorKim, W.G.-
dc.contributor.authorUm, K.-K.-
dc.contributor.authorKim, K.-S.-
dc.contributor.authorLee, S.-
dc.date.accessioned2018-06-15T05:50:00Z-
dc.date.available2018-06-15T05:50:00Z-
dc.date.created2017-12-21-
dc.date.issued2017-06-
dc.identifier.issn0921-5093-
dc.identifier.urihttps://oasis.postech.ac.kr/handle/2014.oak/50893-
dc.description.abstractIn order to understand and improve fracture toughness of heat affected zones (HAZs) of high-strength low alloy (HSLA) steels, complex microstructures including quasi-polygonal ferrite (QPF), acicular ferrite (AF), granular bainite (GB), bainitic ferrite (BF), and martensite-austenite (MA) constituent should be identified, quantified, and then correlated with critical crack tip opening displacement (CTOD). In this study, microscopic analysis methods were achieved for identification and quantitation of microstructures in the HAZs of three HSLA steels. The coarse-grained HAZ (CGHAZ) consisted of AF, GB, and BF together with a small amount of MA, while the inter-critically heated HAZ (ICHAZ) consisted of QPF, GB, and MA. In the CGHAZ, Ni promoted the formation of AF, while it prevented the formation of GB, and the addition of Ni resulted in very high critical CTOD. In the CGHAZ, both Ni and Mn promoted the formation of AF and prevented the formation of GB, while Ni was more effective than Mn. Thus, the addition of Ni resulted in very high critical CTOD. In the ICHAZ, both Ni and Mn promoted the formation MA. However, in the high-Ni-containing steel, a number of MAs were densified along Ni-segregated bands, and thus readily provided void initiation sites. This played an important role in reducing the mean free path for coalescence of voids and crack propagation, which easily led to the serious deterioration of critical CTOD. ? 2017 Elsevier B.V.-
dc.languageEnglish-
dc.publisherElsevier Ltd-
dc.relation.isPartOfMaterials Science and Engineering A-
dc.subjectAlloy steel-
dc.subjectBainite-
dc.subjectCorrosion-
dc.subjectCrack propagation-
dc.subjectCrack tips-
dc.subjectCracks-
dc.subjectFerrite-
dc.subjectFracture toughness-
dc.subjectHigh strength alloys-
dc.subjectHigh strength steel-
dc.subjectManganese-
dc.subjectMartensitic steel-
dc.subjectMicrostructure-
dc.subjectNickel-
dc.subjectCoarse-grained-
dc.subjectComplex microstructures-
dc.subjectCrack tip opening displacement-
dc.subjectCritical crack tip opening displacement-
dc.subjectHigh strength low alloy steels-
dc.subjectInter-critically heated HAZ-
dc.subjectMicroscopic analysis-
dc.subjectSimulated heataffected zones (HAZ)-
dc.subjectHeat affected zone-
dc.titleEffects of Ni and Mn addition on critical crack tip opening displacement (CTOD) of weld-simulated heat-affected zones of three high-strength low-alloy (HSLA) steels-
dc.typeArticle-
dc.identifier.doi10.1016/j.msea.2017.04.115-
dc.type.rimsART-
dc.identifier.bibliographicCitationMaterials Science and Engineering A, v.697, pp.55 - 65-
dc.identifier.wosid000403517400007-
dc.date.tcdate2019-02-01-
dc.citation.endPage65-
dc.citation.startPage55-
dc.citation.titleMaterials Science and Engineering A-
dc.citation.volume697-
dc.contributor.affiliatedAuthorLee, S.G.-
dc.contributor.affiliatedAuthorLee, S.-
dc.identifier.scopusid2-s2.0-85018790785-
dc.description.journalClass1-
dc.description.journalClass1-
dc.description.wostc6-
dc.type.docTypeArticle-
dc.subject.keywordPlusELECTRON BACKSCATTER DIFFRACTION-
dc.subject.keywordPlusLOW-CARBON-
dc.subject.keywordPlusTHERMAL CYCLES-
dc.subject.keywordPlusMECHANICAL-PROPERTIES-
dc.subject.keywordPlusMICROALLOYED STEELS-
dc.subject.keywordPlusACICULAR FERRITE-
dc.subject.keywordPlusLINEPIPE STEELS-
dc.subject.keywordPlusAPI X70-
dc.subject.keywordPlusMICROSTRUCTURE-
dc.subject.keywordPlusSTRAIN-
dc.subject.keywordAuthorHeat affected zone (HAZ)-
dc.subject.keywordAuthorHigh-strength low alloy (HSLA) steel-
dc.subject.keywordAuthorCrack tip opening displacement (CTOD)-
dc.subject.keywordAuthorCoarse-grained HAZ-
dc.subject.keywordAuthorInter-critically heated HAZ-
dc.relation.journalWebOfScienceCategoryNanoscience & Nanotechnology-
dc.relation.journalWebOfScienceCategoryMaterials Science, Multidisciplinary-
dc.relation.journalWebOfScienceCategoryMetallurgy & Metallurgical Engineering-
dc.description.journalRegisteredClassscie-
dc.description.journalRegisteredClassscopus-
dc.relation.journalResearchAreaScience & Technology - Other Topics-
dc.relation.journalResearchAreaMaterials Science-
dc.relation.journalResearchAreaMetallurgy & Metallurgical Engineering-

qr_code

  • mendeley

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher

이성학LEE, SUNG HAK
Dept of Materials Science & Enginrg
Read more

Views & Downloads

Browse